rasman06
New Hunter
My first time.
Sanded with 400 dry
Primed with Rustoleum 2x. Waited 30 hrs
Wet sanded with 1,000 - waited 12 hrs
Used my hands with rub n buff silver leaf

My armor looks like this. Is that how it is supposed to look. I see some swirl marks. Did I use to much? Not enough? Can I recoat?
The tube had a 2014 date on it. Just ordered last week.



Any advice please.
Sent from my iPhone
Sanded with 400 dry
Primed with Rustoleum 2x. Waited 30 hrs
Wet sanded with 1,000 - waited 12 hrs
Used my hands with rub n buff silver leaf

My armor looks like this. Is that how it is supposed to look. I see some swirl marks. Did I use to much? Not enough? Can I recoat?
The tube had a 2014 date on it. Just ordered last week.



Any advice please.
Sent from my iPhone