Reply to thread

My first time. 


Sanded with 400 dry

Primed with Rustoleum 2x. Waited 30 hrs

Wet sanded with 1,000 - waited 12 hrs


Used my hands with rub n buff silver leaf

[ATTACH]51084[/ATTACH]


My armor looks like this. Is that how it is supposed to look. I see some swirl marks. Did I use to much? Not enough? Can I recoat?


The tube had a 2014 date on it. Just ordered last week.


[ATTACH]51085[/ATTACH][ATTACH]51086[/ATTACH][ATTACH]51087[/ATTACH]


Any advice please.





Sent from my iPhone