Ok,

I've had this fiberglass helmet for right at a year and have been to freeked out to paint it. About a month ago I started to do a layered job on it. Well to make the story short I primed, shot silver, dull cote, drew ALL the damage on the dome, masked with mustard. BAD IDEA to use mustard with dull cote........stained all the nice silver damage yellow, name brand mustard I might add. So, sanded it all back down, primed, shot silver, drew on all the damage on the dome, masked with Winsor and Newtons cool.......taped off the dome and sprayed the cheeks.......the paint blistered, Ummm WTF ?


So I pulled of the tape used to mask off the dome...AAARRRRRGGGGGG :angry  !!! That pulled the paint off the dome. (sigh , insert VERY bad four letter word at the top of your lungs).So again I sanded it all down and primed it AGAIN.

Now the PRIMER is blistering !!!!!!!!!!!!!!!!!!! :( :facepalm :angry :puke .

I'm asking for help cause I'm lost.

What do I do now. The primer is blistering in the same spots as the paint before and in NEW spots.


TDH......your my only hope

-Tim-


This thread is more than 18 years old.

Your message may be considered spam for the following reasons:

  1. This thread hasn't been active in some time. A new post in this thread might not contribute constructively to this discussion after so long.
If you wish to reply despite these issues, check the box below before replying.
Be aware that malicious compliance may result in more severe penalties.
Back
Top