So I'm going the sintra route. I've cut out all the pieces I need, but forming them is the biggest pain in the ass I've encountered in this project so far. for example, with the chest armor, I heated each piece in the oven individually until soft and pliable. As many have suggested, I molded these pieces against my torso and then cooled them in cold water. I've done this about four times now, and each time they come out a little lumpy. is my technique screwed up or will i need to sand these to even out the outter surface?
 
I used the boiling water technique.The pot I had wasnt large enough to dip the whole piece, so did it in parts.I did notice that if I didnt heat it up enough, it would leave ripples in the bend.My suggestion if you use the boiling water technique, is to heat it up to where the sintra is floppy.
 
This thread is more than 19 years old.

Your message may be considered spam for the following reasons:

  1. This thread hasn't been active in some time. A new post in this thread might not contribute constructively to this discussion after so long.
If you wish to reply despite these issues, check the box below before replying.
Be aware that malicious compliance may result in more severe penalties.
Back
Top