What should I use to get a good polish on my cold cast parts from MS? I sanded them down with the 600 grit and then hit them with Never Dull but the result is still not very metalic. :confused
 
I used wetsand paper, went from 220 to 1200 grit sanding in one direction only. I then did 1200 grit again with Mothers Mag and Aluminum Polish, then polished again with a soft rag. It wasn't a perfect aluminum finish, but it's the best I could get. I would suggest not using a clearcoat, that may actually dull it down.
 
I've had disapointing results with everything other than wire wool, working with the 0000 grade in one direction seems to give good results...Oh and remember that it will oxidise with time so i suppose some sort of laquer will be required...
 
This thread is more than 17 years old.

Your message may be considered spam for the following reasons:

  1. This thread hasn't been active in some time. A new post in this thread might not contribute constructively to this discussion after so long.
If you wish to reply despite these issues, check the box below before replying.
Be aware that malicious compliance may result in more severe penalties.
Back
Top